Packaging Details: |
Export standard package :bundled wooden box or be required
For 2205 stainless steel sheet price per kg |
---|---|
Delivery Detail: | 15--30 DAYS |
2205 is a duplex (austenitic-ferritic) stainless steel containing about 40 - 50% ferrite in the annealed condition. 2205 has been a practical solution to chloride stress corrosion cracking problems experienced with 304/304L or 316/316L stainless.
The high chromium, molybdenum and nitrogen contents provide corrosion resistance superior to 316/316L and 317L stainless in most environments.
2205 is not suggested for operating temperatures up to 600°F.
The design strength of 2205 is significantly higher than 316/316L, often permitting lighter wall construction.
2205 has good notch impact toughness down to temperatures below - 40°F. 2205 is welded with E2209 or ER2209 fillers.
|
Ni |
Cr |
Mo |
Mn |
Si |
C |
N |
S |
P |
Fe |
MIN |
4.5 |
22.0 |
3.0 |
- |
- |
- |
0.14 |
- |
- |
- |
MAX |
6.5 |
23.0 |
3.5 |
2.0 |
1.0 |
0.03 |
0.2 |
0.02 |
0.03 |
Balance |
2205 Coil, 2205 Pipe, 2205 Plate, 2205 Sheet, 2205 Welding Products
Density:
0.278 lb/inch
3
Melting Point:
2525- 2630°F
Poisson's Ratio:
0.3
Electrical Resistivity:
481 Ohm - circ mil/ft
Temperature, °F |
70 |
212 |
392 |
572 |
Coefficient* of Thermal Expansion, in/in°F x 10 -6 |
- |
8 |
8 |
8 |
Thermal Conductivity
|
8 |
9 |
10 |
11 |
Modulus of Elasticity, Dynamic psi x 10 6 |
28 |
26 |
25 |
24 |
* 70°F to indicated temperature.
Minimum Specified Properties, ASTM A 240
Ultimate Tensile Strength, ksi |
95 |
0.2% Yield Strength, ksi |
65 |
Elongation, % |
25 |
Hardness MAX, Brinell |
290 |
Minimum Elevated Tensile Properties, Plate
Temperature, °F |
212 |
302 |
392 |
482 |
Ultimate Tensile Strength, ksi |
86 |
83 |
80 |
78 |
0.2% Yield Strength, ksi |
52 |
49 |
46 |
44 |
|
PRE n |
Critical Pitting Temperature, CPT |
2205 |
34 |
130°F |
316L |
24 |
62°F |