>> Bisphenol-A epoxy vinyl ester resin
1. Medium-viscosity, non-prepromoted bisphenol-A epoxy vinyl ester resin;
2. Modified by methyl acrylic,
excellent resistance to chemical corrosion
, good
mechanical properties, low shrinkage;
3. Applied in a wide range of FRP applications, especially provides resistance to organic and inorganic acids, alkalis, salt solution, oxidizing chemicals, bleaches and organic solvents;
4. Anti-corrosive level: similiar with
Ashland Derakane 411 /
Swancor 901
>> Applications
1. Pultrusion Profiles, Molded Grating, electrical insulation products, FRP tank, pipe, cooling tower
2. Suitable
for: hand lay up / filament winding / RTM / Spray Up, mix with Glass-Flake, filled linings
>> Package & Delivery
Weight/Drum: 200kg
Drums/Pallet: 4
Qty/40'Fcl: 120drums/40'Fcl, 24,000kg
Qty/20'Fcl: 80drums/20'Fcl, 16,000kg
>> Tech Data Sheet & MSDS
Typical Room-Temperature Properties
(1)
of Postcured
(2)
4mm Resin Castings
Item
|
Value
|
Test method
|
Tensile Strength (MPa)
|
85
|
GB/T 2568-1995
|
Tensile Modulus (Gpa)
|
3.3
|
GB/T 2568-1995
|
Tensile Elongation (%)
|
4.0~6.0
|
GB/T 2568-1995
|
Flexural Strength (MPa)
|
140
|
GB/T 2570-1995
|
Flexural Modulus (MPa*10
3
)
|
3.4
|
GB/T 2570-1995
|
Un-notched Impact Strength (KJ/m
2
)
|
13.2
|
GB/T 2571-1995
|
Heat Distortion Temperature (°C, at 1.82 MPa applied stress by Vicat HDT)
|
120
|
GB/T 1634-1989
|
Barcol Hardness
|
42
|
GB/T 3854-1983
|
Vol
ume Curing Shrinkage
,(%)
|
7.5
|
JB/T 6542-1993
|