Tungsten carbide inserts
Use large-grain coarse-grained tungsten carbide, which has high wear resistance, impact resistance and thermal stability
Shank body
High-quality alloy steel is selected, and the stable heat treatment process makes the tooth body wear-resistant and tough
Brazing process
Through special welding process, the strength of pick welding is increased, the impact resistance is improved, and the carbide tip is not easy to fall off
Shank reinforcement
Through laser cladding, powder metallurgy technology and other technologies to protect the head of the tooth body, reduce the wear rate and extend the service life
(mm) | ||||||||
Model |
Carbide diameter (D1) |
Body diameter (D2) |
Clip daimeter (D3) |
Clip width | Clip location | Holder length | Body length | Type |
DMT3050 | 16-22 | 50 | 30 | 38 | / | 70-90 | 130-150 | Rotary picks |
DMT3055 | 19-30 | 55 | 30 | 38 | / | 75 | 135 | Rotary picks |
DMT 3060 | 19-30 | 60 | 30 | 38 | / | 73-92 | 133-152 | Rotary picks |
DMT U84 | 16-22 | 30 | 26 | 28 | 65.5 | 80 | 152 | Coal picks |
DMT U92 | 16-22 | 35 | 30 | 28 | 82 | 102 | 196 | Coal picks |
DMT U94 | 19-25 | 35 | 30 | 28 | 82 | 90 | 184 | Coal picks |
DMT U95 | 22-30 | 35 | 30 | 28 | 82 | 90 | 184 | Coal picks |
DMT U170 | 22-30 | 43 | 35 | 30 | 28 | 112 | 102 | Coal picks |
HWMJS135 | 19-30 | 38 | 35 | 5 | 70 | 80 | 80 | Road header picks |
HWMCU47 | 16-25 | 38 | 30 | 26 | 7 | 70.5 | 71 | Road header picks |