Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron

Model NO.
14~20%
Usage
Steel Making
Melting Temperature
1400-1550
Density
5.8-6.5g/cm3
Sample
Avaiable
MOQ
1kg
Appearance
Silver Metal Block
Materials
Feb
CAS
11108-67-1
Size
10-100mm
Transport Package
50kg Drum
Specification
14~20%
Trademark
Fitech
Origin
China
HS Code
7202999900
Production Capacity
100mt/Year
Reference Price
$ 720.00 - 900.00

Product Description

Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron
Ferro Boron
1.  Molecular formula: FeB

2. Melting Point: 1400~1550ºC

3. CAS No.: 12604-58-9

4. HS Code: 7202999900

 
5.  Purity: 14~20%
Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron       Alloy of boron and iron.  According to carbon content, boro-iron (boron content: 5-25%) can be divided into low carbon (C≤0.05% ~ 0.1%,9% ~ 25%B) and medium carbon (C≤2.5%,4% ~ 19%B). Iron boron is a strong deoxidizer and boron addition agent in steelmaking. The greatest role of boron in steel is that only a very small amount of it can significantly improve the hardenability and replace a large number of alloying elements. In addition, it can also improve mechanical properties, cold deformation properties, welding properties and high temperature properties.
 
    Mainly used in steel and cast iron. Used for alloy structural steel, spring steel, low alloy high strength steel, heat resistant steel, stainless steel, etc. Boron can improve toughness and wear resistance in cast iron, and is widely used in the manufacture of automobile, tractor and machine tool.
 
Product name
Ferro Boron
Grade
Industrial Grade
Color
Grey with Metallic Luster
Purity
14~20%
Shape
Lump
  Density   5.8-6.5g/cm3
Melting Point
1400-1550ºC
 
Applications
    Adding 0.07%B to steel can significantly improve the hardenability of steel. Boron added to 18%Cr, 8%Ni stainless steel after treatment can make precipitation hardening, improve high temperature strength and hardness. Boron in cast iron will affect the graphitization, thus increasing the depth of the crack to make it hard and wear resistant. Adding 0.001% ~ 0.005% boron to malleable iron is beneficial to forming spheroidal ink and improving its distribution. Low aluminum and low carbon boron iron are the main raw materials of amorphous alloys.
Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron

Related Products
                                                Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron
                                                                Ferro Molybdenum                                                                                               Ferro Silicon

Packing
Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron

Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron                                                                                       
Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron
 
Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron

Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron
Used for Smelting Alloy Steel Boron Iron 10~100mm 14~20% Ferro Boron
Q: Are you trading company or manufacturer ?
A: We are factory.

Q: How long is your delivery time?
A: Generally it is 5-10 days if the goods are in stock. or it is 15-20 days if the goods are not in stock, it is according to
quantity.

Q: Do you provide samples ? is it free or extra ?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.

Q: What is your terms of payment ?
A: Payment<=1000USD, 100% in advance. Payment>=1000USD, 30% T/T in advance ,balance before shippment.