Introduction
Stainless Steel Square Tube has greater strength and superior corrosion resistance. The ISO 9001 management system ensure the high quality of the products.
Application
The products are used to construct high pressure and ultra high pressure power station boilers, superheated steam pipes, boiling water pipes and superheated steam pipes for locomotive boilers. Fourth, special pipe technology
Internal and external polishing (surface grade: polishing 180 #, 220 #, 240 #, 320 #, 400 #, 600 #); wire drawing; pickling; leveling of the inner bead; online bright heat treatment.
Specification
Name | 300 Series Stainless Steel Welded High Precision Square And Rectangular Pipe | |||||
Standard | GB12770,GB12771,ASTM A249,ASTM A269,ASTMA270,ASTMA312,ASTMA554,JIS G 3463 | |||||
Material Grade | 304,316,201,202,316L,430 | |||||
Main Material | a) 201 (Ni0.8%-1%) | |||||
b) 202 (Ni: 3.5%-4.5%) | ||||||
c) 304 (Ni: 8% Cr: 18%) | ||||||
d) 316 (Ni: 10% Cr: 18%) | ||||||
Thickness | 0.5-2.0mm | |||||
Length | 15x15,18x18,20x20,23.5x23.5 or as customers' request | |||||
Tolerance | a)Outer Diameter; +/-0.2mm | |||||
b)Thickness; +/-0.03mm | ||||||
c)Length;+/-5mm | ||||||
Surface | 180G, 320G, 400G Satin / Hairline | |||||
400G, 500G, 600G or 800G Mirror finish | ||||||
Application | Electronics | |||||
Test | Squash test, extended test, water pressure test, crystal rot test, heat treatment, NDT | |||||
Chemical Composition of Material | Composition | 201 | 202 | 304 | 316 | 430 |
C | ≤0.15 | ≤0.15 | ≤0.08 | ≤0.08 | ≤0.12 | |
Si | ≤1,00 | ≤1,00 | ≤1,00 | ≤1.00 | ≤1.00 | |
Mn | 5.5-7.5 | 7.5-10 | ≤2.00 | ≤2.00 | ≤1.00 | |
P | ≤0.06 | ≤0.06 | ≤0.045 | ≤0.045 | ≤0.040 | |
S | ≤0.03 | ≤0.03 | ≤0.030 | ≤0.030 | ≤0.030 | |
Cr | 12.5-14.5 | 15-18 | 18-20 | 16-18 | 16-18 | |
Ni | 0.8-1.5 | 46 | 8-10.5 | 1014 | ||
Mo | 2.0-3.0 | |||||
Mechanical Proper | Material Item | 201 | 202 | 304 | 316 | |
Tensile Strength | ≥535 | ≥520 | ≥520 | ≥520 | ||
Yield Strength | ≥245 | ≥205 | ≥205 | ≥205 | ||
Extension | ≥30% | ≥30% | ≥35% | ≥35% | ||
Hardness(HV) | <253 | <253 | <200 | <200 |