Test Method | Property | Unit | Standard | Result |
GB/T 13477 (ISO 7390) | Slump (vertical) | mm | ≤3 | 0 |
GB/T 13477 (ISO 8394) | Extrusion Rate | ml/min | ≥80 | 415 |
GB/T 13477 (ASTM D 2377) | Tack Free Time | h | ≤3 | 0.8 |
GB/T 13477 (ISO 7389) | Extension Recovery | % | ≥80 | 86 |
GB/T 13477 (ISO 10563) | Weight Loss | % | ≤8 | 6 |
GB/T 13477 (ISO 8339) | Tensile Modulus | MPa | >0.4 | 0.7 |
GB/T 13477 (ISO 11600) | Movement Capability | % | ± 20 | ± 20 |
JC/T 485 | Adhesion after UV Exposure | No Failure | ||
GB/T 13477 (ISO 8340) | Adhesion at fixed stretch | |||
GB/T 13477 (ISO 9047) | Adhesion after heat contract and cold extension | |||
GB/T 13477 (ISO 10590) | Adhesion after water immersion |