ASTM/ASME | JIS | En | DIN | C | Cr | Ni | Mo | Others | Remark |
N10276 | QA C276 | 2.4819 | 0.010 | 14.5~16.5 | Balance | 15.0~17.0 |
Straight/U
Bend |
||
N06455 | 2.4610 | 0.010 | 14.0~18.0 | Min.65 | 14.0~17.0 | Ti: MAX.0.70 |
Straight/U
Bend |
||
N06600 | NCF600 | NiCr15Fe | 0.150 | 14.0~17.0 | Min.72 | Cu:MAX.0.50 |
Straight/U
Bend |
||
N06625 | 2.4856 | 20.0~23.0 | Min.58 | 8.0~10.0 | Cu:MAX.0.50 | Straight | |||
N04400 | QA625 | 2.4360 | NiCu30 | 0.300 | 17.5~19.5 | Min.63 | Cu:28.0~34.0 |
Straight/U
Bend |
Corrosion Test | Conducted only when specially requested by the client |
Chemical Analysis | Test done as per required quality standards |
Destructive / Mechanical Testing | Tensile | Hardness | Flattening | Flare | Flange |
Reverse-bend and Re. flat tests | Carried out in full compliance with relevant standards & ASTM A-450 and A-530 norms, which ensures trouble-free expansion, welding & use at customers end |
Eddy Current Testing | Done to detect homogeneities in subsurface by using Digital Flaw-mark Testing System |
Hydrostatic Testing | 100% Hydrostatic Testing carried out according to ASTM-A 450 norms for checking tube leakage, and biggest pressure we can support 20Mpa/7s . |
Air Under Pressure Test | To check any evidence of air leakage |
Visual Inspection | After passivation, every single length of tubes & pipes is subjected to thorough visual inspection by trained staff for detecting surface flaws & other imperfections |
Eddy Current Testing
O.P Testing Radiography Testing |
Corrosion Testing
Micro Testing Macro Testing |
IGC Testing
Ultrasonic testing Liquid Penetrate testing |