Low Price 1.4571/ (X6CrNiMoTi17- 12 -2) Heat-Resistant Staninless Steel Plate

Model NO.
1.4571
Surface Treatment
Polished
Types
Stainless Steel Plate
Applications
Industrial, Construction, Decorative
Grades
DIN 1.3805 X35mn18 Hot Rolled Steel
Techniques
Hot Rolled, Cold Rolled Hot Rolled
Special Use
Austenitic, Non-Magnetic Mn-Steel
Surface
Polished
Surface Treatments
Coated
Shipping
Air; Sea
Delivery Time
5-30 Days
Width
200-150mm
Transport Package
Water-Proofed Bags or Standardized Wooden Case
Specification
Length: 2000*6000mm
Trademark
Bozhong
Origin
Shanghai
HS Code
7219210000
Production Capacity
5000ton/Month
Reference Price
$ 890.10 - 1,260.00

Product Description

Low Price 1.4571/(X6CrNiMoTi17-12-2)Heat-Resistant Staninless steel plate
 
1.Product Description

Stock 316Ti stainless steel sheet S31635 1.4571
EN 1.4550 - 347 is a high alloy austenitic stainless steel with low carbon content. The grade is intended for use under severe corrosive conditions. The steel grade was originally developed to resist corrosion in dilute sulphuric acid. EN 1.4550 is fully austenitic, and is less sensitive to precipitation of ferrite and sigma phase than conventional austenitic grades with high molybdenum content. Due to the combination of relatively high contents of chromium, nickel, molybdenum and copper,   EN 1.4550 has good resistance to general corrosion, particulary in dilute sulphuric acid.  It is non-magnetic in the annealed condition but may become slightly magnetic as a result of cold-working or welding.
Design features  
⇒ Good resistance to uniform corrosion
⇒ Good resistance to pitting and crevice corrosion  
⇒ Very good resistance to stress corrosion cracking
⇒ Good resistance to intercrystalline corrosion
⇒ Good formability and weldability
Corrosion resistance  
Uniform corrosion Uniform corrosion is characterized by a uniform corrosion of the steel surface in contact with the corrosive medium. Resistance is normally considered good if the corrosion rate is less than 0,1 mm/year. As a result of its high chromium, nickel and molybdenum contents and its alloying with copper, EN 1.4550 is passivated even in reducing environments such as dilute sulphuric acid and formic acid. Its high nickel content contributes towards its relatively low corrosion rate in the active state.  
Intercrystalline corrosion  
EN 1.4550 has a very low carbon content. This means that there is very little risk of carbide precipitation in connection with ordinary heat treatment and welding. The risk of intercrystalline corrosion after ordinary heat treatment and welding is thereby eliminated.

Low Price 1.4571/ (X6CrNiMoTi17-12-2) Heat-Resistant Staninless Steel Plate

Low Price 1.4571/ (X6CrNiMoTi17-12-2) Heat-Resistant Staninless Steel Plate
Low Price 1.4571/ (X6CrNiMoTi17-12-2) Heat-Resistant Staninless Steel Plate
Low Price 1.4571/ (X6CrNiMoTi17-12-2) Heat-Resistant Staninless Steel Plate



 
Stainless steel maintenance

(1) Regular cleaning and maintenance
(2) Pay attention to prevent the occurrence of the phenomenon of surface scratches
(3) Use soap, weak detergent or warm water to remove surface dust, dirt
(4) In addition to the surface of the binder with alcohol or an organic solvent (ether, benzene)
(5) Use neutral detergent or ammonia solution in addition to surface oil
(6) With 10% nitric acid or abrasive detergent in addition to the surface of the embroider caused by the dirt.



FAQ

Q: Are you a manufacturer or merely a trader?
A: We are group of companies and owned manufacturer bases and trading company. We specialized in special steel which include alloy structural steel and carbon steel and stainless steel, etc. All material are with high quality and competitive price.

 
Q: How do you guarantee the quality of your product?
A: Firstly, we can provide the certificates from the third party, such as TUV, CE, if you need. Secondly, we have a complete set of inspection system and every process is checked by QC. Quality is the lifeline of enterprise survival.

Q: Delivery time?
A: We have ready stock for most of material grades in our warehouse. If the material don't have stock, the delivery lead time is about 5-30 days after receiving your prepayment or firm order.
 
Q: What is the payment term?
A: T/T or L/C.

Q: Can you provide a sample for our testing before confirm the order?
A: Yes. We can provide sample to you for approval before you place an order to us. Free sample is available if we have stock.
 
Q: Can we visit your company and factory?
A: Yes, warmly welcome! We can book the hotel for you before you come to China and arrange our driver to our airport to pick you up.
 
Low Price 1.4571/ (X6CrNiMoTi17-12-2) Heat-Resistant Staninless Steel Plate
Low Price 1.4571/ (X6CrNiMoTi17-12-2) Heat-Resistant Staninless Steel Plate




4. Contact us

Name: Denny Cheng
Direct line: 021-67897611

Address: 518,XINZHUAN ROAD, SONGJIANG DISTRICT, SHANGHAI, CHINA 201612