High density polyethylene (HDPE), white powder or granular product. Non-toxic, tasteless, crystallinity of 80% ~ 90%, softening point of 125 ~ 135ºC, use temperature up to 100ºC; The hardness, tensile strength and creep properties are better than those of LDPE. Good wear resistance, electrical insulation, toughness and cold resistance; Good chemical stability, at room temperature, insoluble in any organic solvent, acid, alkali and various salts corrosion ; The membrane has low permeability to water vapor and air and low water absorption. Poor aging resistance, environmental stress cracking resistance is not as good as low density polyethylene, especially thermal oxidation will make its performance decline, so the resin must be added to the antioxidant and ultraviolet absorbent to improve the lack of this aspect. High density polyethylene film has low thermal deformation temperature under stress, so attention should be paid to its application.
Item | Unit | Test method |
Density | 0.954 g/cm 3 | ASTM D1505 |
Melt Index (190 °C /2.16kg) | 0.9 g/10 min | ASTM D1238 |
Falling Weight Impact Strength | 50g | ASTM D1709 |
Elmendorf Tear Strength | 10kg/cm | ASTM D1922 |
Film Impact Strength
|
160kg.cm/mm | ASTM D3420 |
Youngs Modulus | 600/750MPa | ASTM D882 |
Tensile Strength(YIELD) | 70/60MPa | ASTM D882 |
Tensile Strength(break) | 30/30MPa | ASTM D882 |
Elongation(break) | 650/750MPa | ASTM D882 |
V icat T emperature | 129 °C | ASTM D1525 |
Low temperature brittleness | -70 °C | ASTM D746 |
Melt Temperature | 180-220 °C |
|
Acid and alkali resistance, organic solvent resistance, excellent electrical insulation, low temperature, still can maintain a certain toughness. Surface hardness, tensile strength, rigidity and other mechanical strength are higher than LDPE, close to PP, tougher than PP, but the surface finish is not as good as PP.
Poor mechanical performance, poor air permeability, easy deformation, easy aging, easy to brittle, brittle than PP, easy to stress cracking, low surface hardness, easy to scratch. Difficult to print, printing, need to carry out surface discharge treatment, can not electroplate, surface dull.
Used for extruding packaging film, rope, woven bag, fishing net, water pipe; Injection molding low-grade daily necessities and shells, non-load-bearing components, plastic boxes, turnover boxes; Extrusion blow - molded containers, hollow products, bottles.
1. What is your terms of packing?
Generally, we pack our goods in carton with pallet. |
2.What is your tems of payment?
T/T 30% as deposit, and 70% before delivery. We'll show you the photos of the products and packages before you pay the balance. |
3. What is your terms of delivery?
EXW, FOB, CFR, CIF,L/C at sight |
4. How about your delivery time?
Generally, it will take 21 days after receiving your advance payment. The specific delivery time depends on the items and the quantity of your order. |
5. Can you produce according to the samples?
Yes, we can produce by your samples or technical drawings. We can build the molds and fixtures. |
6. What is your sample policy?
We can supply the sample if we have ready parts in stock, but the customers have to pay the sample cost and the courier cost. |
7. Do you test all your good before delivery?
Yes, we have 100% test before delivery . |