Tensile Strength MPa
42.5-44.8
Specific Heat Capacity(J/Kg.K)
900
Flexural Strenght(MPa)
60.6-73.1
Flexural Modulus(Gpa))
2.25-2.28
Modulus of Elasticity(Gpa)
2.0-2.6
Glass Transition Temperature
105
Coefficient of Thermal Expansion
120
Thermal Conductivity (W/M.K))
0.1
Specification
According to drawing
Production Capacity
10000PCS/Month